金属胶接固化过程中,胶膜在高温高压下融化流动,多余胶液受挤压排出,造成零件局部溢胶过多,胶瘤尺寸过大,影响制件的最终装配。通过分析胶液流动固化后体积变化,开展高度和间隙补偿等对溢胶面积及胶瘤尺寸进行控制的工艺研究。研究结果表明:在固化温度及压力一定的情况下,胶接固化溢胶量基本相同;通过模具优化可改变溢胶扩展规律,有效减小装配区胶接溢胶量,实现零件表面溢胶面积及胶瘤尺寸的控制。
Abstract:In the process of metal bonding and solidification,adhesive film melted and flowed under high temperature and high pressure,and excess adhesive solution was squeezed out. As a result,it caused excessive adhesive overflow in parts and relatively large size of adhesive fillet,which influenced the final assembly of parts.Based on the analysis of volume change of adhesive solution after flowing and solidifying,the research on the control technology of height and gap compensation on the overflow area and adhesive fillet size was carried out. The research results showed that under the condition of certain curing temperature and pressure,the amount of adhesive overflow was basically the same. The expansion rule of adhesive overflow could be changed through mold optimization,which could effectively reduce the amount of adhesive overflow in the assembly area,and achieve the control of adhesive overflow area and adhesive fillet size on the surface of parts.
[1]谢富原,王雪明,李敏,等.T形加筋板热压罐成型过程压力分布与树脂流动实验研究[J].复合材料学报,2009,26(6):66-71.
[2]余海洲,赵迪,李阳.胶瘤入射角度对单搭胶接接头拉剪强度和应力分布的影响[J].机械工程材料,2016,40(7):60-63.
[3]乔海涛,梁滨,张军营,等.先进复合材料结构胶接体系的研发与应用[J].材料工程,2018,46(12):38-47.
[4]COGNARD P.Adhesives and sealants-basic concepts and high tech bonding[M].Kidlington:Elsevier Ltd.,2005:303-321.
[5]韩啸,金勇,杨鹏.结构胶接接头湿热环境耐久性研究概述[J].河北科技大学学报,2017,38(3):209-217.
[6]江乐彬,谢惠民,王怀喜,等.单搭接胶接接头拉伸剪切性能的数值模拟与实验研究[J].实验力学,2012,27(6):643-649.
[7]何凯,龚志红,徐娟,等.FM73M胶膜及其与PMI泡沫芯的胶接机理[J].宇航材料工艺,2013,43(1):82-85.
[8]孙文智,李承昌.环氧树脂胶液在混凝土裂缝中的流动研究[C].浙江省公路学会2005年年会论文集,杭州,2006.
[9]张艳芳,冷卫红,罗辑,等.复材/复材二次胶接胶接质量及强度影响因素研究[J].塑料工业,2014,42(7):77-80.
[10]周文玉,郭健明,李菊丽.模具高精度数控加工的探讨[J].轻工机械,2005,23(4):84-87.32
基本信息:
DOI:10.13416/j.ca.2020.05.003
中图分类号:TG49;V261
引用信息:
[1]彭坚,陈翠,吕云飞等.金属胶接胶瘤尺寸控制[J].中国胶粘剂,2020,29(05):6-9+32.DOI:10.13416/j.ca.2020.05.003.
基金信息: